Specifikation
Produktnavn | Spiral svejset stålrør |
Standard | API5L, ASTM A106 GR.B, ASTM A53 GR.B, ASTM A270, ASTM A249, ASTM A511, ASTM A778, ASTM A312, ASTM A358, ASTM A409, ASTM A213, ASTM A790, ASTM A268, ASTM A554, ASTM B338, ASTM B673, ASTM B674, ASTM B677, ASTM B675, ASTM B676, ASTM B690, ASTM A928, ASME B36.19, ASMEB36.10, ASTMA179/A192/A213/A210/370WP91, WP11, WP2GB5310-2009, GB3087-2008, GB6479-2013, GB9948-2013, GB/T8163-20088, GB8162-2008, GB/T17396-2009EN10216-5, EN10217-7, DIN 17456, DIN 17458 JIS G3463, JIS G3119, JIS G3446, JIS G3218, JIS G3258, JIS G3448, JIS H4631P 32, DNV-OS-F101 |
Grad | Q195 = S195 / A53 klasse AQ235 = S235 / A53 Grad B / A500 Grade A / STK400 / SS400 / ST42.2Q345 = S355JR / A500 Grade B Grade C |
Ydre diameter | 1/8 - 126 tommer |
Vægtykkelse | 0,4-40 mm |
Længde | 5,8 ~ 12,0 m eller som tilpasset |
Overfladebehandling | Prime kvalitet (spærret, olieret, farvemaling, 3LPE eller anden anti-korrosiv behandling) |
Inspektion | Med kemisk sammensætning og mekanisk egenskabsanalyse; dimensionel og visuel inspektion, også med ikke -destruktiv inspektion. |
Anvendelse
Struktur, elektrisk krafttransmissionstårnprojekter, stabling, vand, olie- og gasrørledningsteknik, mekanisk industri, kommunale projekter, veje og dets hjælpefaciliteter osv.
Mekaniske egenskaber
Stålkvalitet | Udbyttestyrke, min. PSI (MPA) | Tensil styrke, min. PSI (MPA) | Forlængelse i 2 tommer, min. Beholdende | Minimum påvirkning Energi KV J | ||
Ved testtemperatur på | ||||||
-20 | 0 | 20 | ||||
S235JRH | 235 | 360 | 24% | – | – | 27 |
S275JOH | 275 | 430 | 20% | – | 27 | – |
S275J2H | 355 | 510 | 20% | 27 | – | – |
S355JOH | 355 | 510 | 20% | – | 27 | – |
S355J2H | 355 | 510 | 20% | 27 | – | – |
S355K2H | 355 | 510 | 20% | 40 | – | – |